This study investigated the precipitation
strengthening of the binary Al-0.14wt% Sc,
0.16% Ti alloy system. Ingots of Al-2.1wt% Sc
and Al-4.68wt% Ti were melted together, and
the nucleation, growth, and coarsening of
precipitates were analyzed. The microstructural
evolution of the nanoscale L12 precipitates
phase was examined with Vickers
microhardness testing,...
Aluminum alloys strengthened with coherent (L1<sub>2</sub>), nanosize Al<sub>3</sub>Sc precipitates may be used as structural materials at elevated temperatures. They are creep resistant at 300°C and exhibit a threshold stress, below which creep is not measurable. Introducing ternary alloying additions, such as rare-earth elements (RE=Y, Dy, Er), that segregate within Al<sub>3</sub>Sc...